High Purity Fused Cast Zirconia Block RTK-Z9540 from China Suppliers - Ideal for Glass Furnace Applications
Fused cast zirconia blocks are high zirconia refractories made by melting high purity raw materials through special casting process. The series of molten high zirconium bricks mainly includes RTK-Z9540 (zirconium content >89%) and RTK-Z9510 (zirconium content >93%).
RTK-Z9540 Mineral composition: ZrO₂ (89%), SiO₂ (9%), Na₂O (0.05%)
The crystalline structure of fused cast zirconia blocks is mainly composed of baddeleyite, so it has extremely high corrosion resistance and low foaming rate characteristics. These advantages effectively prevent the contamination of the molten glass.
Zirconia refractory products are produced with PLC programmed special electric furnace and special material incubator. During casting, the shrinkage cavity block is obtained after molding. This casting method is generally used for cast zirconia block products.
Fused cast high zirconium brick is one of our four core products. The main physical and chemical indexes of high zirconium brick series products produced by Reftech have reached the level of international mainstream suppliers, and the quality of products can be fully guaranteed.
- Liquid crystal substrate glass furnaces
- High alumina glass furnaces
- Borosilicate glass furnaces
- Halogen lighting glass furnaces
- Glass ceramic & glass fiber furnaces
| Chemical Composition and Mineral Composition | ||
|---|---|---|
| Composition Type | Value (%) | |
| Chemical Composition (%) | ZrO₂ | 89.0 |
| SiO₂ | 9.1 | |
| Al₂O₃ | 1.5 | |
| Na₂O | 0.1 | |
| Others | 0.3 | |
| Mineral Composition | ||
| Mineral Composition (%) | Baddeleyite | 88 |
| Vitreous Phase | 12 | |
| Physical Property | |
|---|---|
| Normal temperature compressive strength (Mpa) | 600 |
| Bulk density (g/cm³) | 5 |
| Apparent porosity (%) | ≤1 |
| Corrosion resistance of molten glass at three-phase interface (mm/24h) | ≤0.8 |
| Exudation amount of vitreous phase | ≤0.4 |
|
Thermal conductivity W/(m·k)
At 600°C
At 1000°C |
3.0 2.8 |
|
Resistivity (Ω·m)
At 1500°C
At 1600°C |
5.0 2.4 |
|
Coefficient of thermal expansion
At 1000°C
At 1500°C |
0.65 0.10 |