Leave Your Message

Fused Cast 41#AZS Block ( RTK-AZS41)

RTK-AZS41 has high corrosion resistance and low pollution to molten glass, and is suitable for parts in glass furnace that require high corrosion resistance, such as fully electric melting furnace, throat, weir, bubbler block, and doghouse corner block. The main chemical composition is SiO₂, Al₂O₃, ZrO₂, and the raw materials are high purity alumina, zircon sand and zirconia, and the reasonable ratio makes the product pure texture and reasonable crystal phase structure and these materials are tested for chemical composition and physical and chemical properties before use

    Berif Introduction

    RTK fused cast AZS blocks are made of high-quality purified raw materials, using a special electric arc furnace, and a fused cast process that has undergone long arc melting and oxidation treatment. This process has almost no carbon contamination from the electrode. Due to the oxidation fused cast process and the use of high-purity raw materials, RTK fused cast AZS series have special and high resistance to the corrosion of molten glass, and have little contamination to the molten glass.
    Fused cast AZS products can be divided into 41# AZS block (RTK-AZS41), 36 # AZS block (RTK-AZS36) and 33 # AZS block(RTK-AZS33) according to the different ZrO₂, content in the chemical composition. In addition, on the basis of RTK-AZS36 and RTK-AZS33 manufacturing processes, the content of corresponding chemical components of Si0₂ and Na₂O has been reduced, and two products, 36 # low silicon low sodium AZS blocks (RTK-AZS36D) and 33 # low silicon low sodium AZS blocks (RTK-AZS33D), have been formed. These five products are further classified according to different casting methods, which can meet the different use requirements of fused cast products in glass furnaces.
    RTK-AZS41 has high corrosion resistance and low pollution to molten glass, and is suitable for parts in glass furnace that require high corrosion resistance, such as fully electric melting furnace, throat, weir, bubbler block, and doghouse corner block.

    Chemical composition

    • AZS#41-2
    • AZS#41-1

    CHEMICAL COMPOSITION

    TYPICAL VALUE

    SiO2% 12
    Al2O3 % allowance
    ZrO2 % 41
    Fe2O3+TiO3+CaO+MgO+Na2O+K2O % ≤2.0

    Physical property

    PHYSICAL PROPERTY

    TYPICAL VALUE

    Bulk density (dense part) g/cm3 4.05
    Apparent porosity (dense part) % 0.6
    Initial precipitation temperature of vitreous phase°C 1400
    Vitreous phase exudation (1500°CX4hr)% 1.5
    Anti-molten glass erosion speed under static condition mm/24hr 1.2
    Bubble release rate%(1300°CX10hr,ordinary soda lime glass) 0.6

    CALCULATE SPECIFIC GRAVITY

    TYPICAL VALUE

    Ordinary casting /inclined casting g/cm3 3.65
    Quasi-non shrinkage casting g/cm3 3.90
    Non shrinkage casting g/cm3 4.00

    Leave Your Message